Filament Drying for PETG, TPU, and Nylon: One Dryer, Three Spools

Plan a drying schedule for PETG, TPU, and nylon when you share one filament dryer. Compare product-specific settings, decide when to dry separately, and keep each spool ready for printing.



By XUCHUN

Filament Drying for PETG, TPU, and Nylon: One Dryer, Three Spools

XUCHUN

Filament Drying for PETG, TPU, and Nylon: One Dryer, Three Spools

You have a PETG bracket to print this afternoon, a TPU bumper to print tomorrow, and a long nylon job after that. You have one filament dryer. Which spool goes in first?

Start by checking the drying instructions for each spool and the temperature limits of your dryer and spool. Then work backward from when each print will start. If the nylon grade needs to feed from the dryer throughout its print, reserve the dryer for both the drying cycle and the print itself.

PETG, TPU, and Nylon Drying Temperatures and Times

Use the row that matches your exact product. These examples show how much the cycle can vary between products, even within the same material family.

Filament Manufacturer’s drying temperature Time Source
INKCLOUD PETG Basic 60 ± 5°C 4–8 hours INKCLOUD PETG Basic
TPU listed in Prusa’s drying guide 60°C 4–6 hours Prusa drying guide
Polymaker PolyFlex TPU95-HF 70°C 8 hours Polymaker technical data sheet
Prusament PA11 Carbon Fiber 90°C 6 hours Prusa drying guide
Polymaker PolyMide CoPA 100°C 8 hours Polymaker CoPA guide

Before starting a cycle, confirm that the dryer can maintain the required temperature and that the reel is rated for it. Follow the dryer’s instructions for airflow, venting, and spool placement. If your dryer tops out at 70°C and your nylon supplier specifies 100°C, ask the supplier whether it has a validated lower-temperature cycle or use equipment rated for the specified cycle. Prusa drying guide

How to Schedule One Dryer Around Three Prints

First slot: PETG for the afternoon bracket

If the PETG spool needs drying, give it the first slot so it is ready for the nearest print. After the cycle, print with it or move it to sealed storage with desiccant. This frees the dryer for the next spool while the bracket prints. INKCLOUD PETG Basic

Second slot: TPU for tomorrow’s bumper

Use the drying cycle for the TPU on your bench. The table shows why copying a setting from another TPU spool can change both the temperature and the time you need to reserve.

If the TPU feeds unevenly after drying, check whether the spool turns freely and whether the filament bends or buckles between the drive gears and hotend. A short, well-constrained filament path can help resolve a feeding problem that another drying cycle would leave unchanged. INKCLOUD printing FAQs

Final slot: Nylon immediately before the long print

Schedule nylon close to the print start to limit its time in room air. Check whether the supplier recommends feeding from a dry box or a heated dryer. Polymaker, for example, recommends keeping CoPA in a heated filament dryer throughout printing. For that workflow, book the dryer until the print ends. Polymaker CoPA guide

Can You Dry PETG and TPU Together?

Yes, if the dryer is designed for multiple spools and the selected temperature and duration fall within the documented guidance for both products and both reels.

For example, 60°C for six hours falls within the published guidance for INKCLOUD PETG Basic and the TPU entry in Prusa’s drying guide. PolyFlex TPU95-HF has a different published cycle. If the two products on your bench have no documented overlap, schedule them separately. INKCLOUD PETG Basic · Prusa drying guide · Polymaker TPU95-HF technical data sheet

How to Tell Whether Drying Helped

Print a small sample before and after drying. Keep the spool, model, nozzle temperature, and slicer profile the same. Compare nozzle popping, bubbles, pits, and surface consistency. Improvement across several of these signs gives you a better reason to suspect moisture than stringing alone. Prusa drying guide

If the surface improves but strings remain, check the material’s nozzle temperature and retraction guidance. If the remaining problem is intermittent under-extrusion, check the spool path and nozzle before booking another drying cycle. INKCLOUD printing FAQs

Can a Dry Box Replace a Filament Dryer?

Use an active dryer to remove moisture from a damp spool. Use sealed storage with desiccant to help protect a dry spool between jobs. If a dryer also has a feed-through port, follow its instructions for feeding filament while printing. A low humidity reading inside a box describes the air near its sensor, while the before-and-after print gives you a practical check on extrusion. Prusa drying guide

For a shared dryer, label each spool with its material, drying cycle, and last drying date. That gives the next person enough information to decide whether to print, store, or dry it again. When buying a replacement spool, check its drying instructions alongside its print settings, especially if your dryer has a limited temperature range. Browse INKCLOUD filaments

Manufacturer guidance checked November 10, 2026.